Poud asye pur fèt pa pwosesis atomizasyon dlo e li gen bon rezistans korozyon ak rezistans.Poud asye pur gen yon pakèt itilizasyon endistriyèl.
Bay yon varyete de poud metal asye pur ak gwosè patikil diferan.
1.Hot izostatik peze
2.Metal piki bòdi
3.3D enprime
4.Thermal flite
1.Atomizasyon dlo
2.Water gaz konbine atomizasyon
3.Atomizasyon gaz
4.Vacuum atomizasyon
Konpozisyon poud asye Stainess % | |||||||||
Klas | Cr | Ni | Mo | Nb | Cu | S | P | C | Si |
303 | 17-19 | 8-13 |
|
|
| 0.15-0.3 | ≤0.2 | ≤0.15 | ≤1 |
304 | 18-20 | 8-12 |
|
|
| ≤0.03 | ≤0.04 | ≤0.08 | ≤1 |
316 | 16-18 | 10-14 | 2-3 |
|
| ≤0.03 | ≤0.04 | ≤0.08 | ≤1 |
303L | 17-19 | 8-13 |
|
|
| 0.15-0.3 | ≤0.2 | ≤0.03 | ≤1 |
304L | 18-20 | 8-12 |
|
|
| ≤0.03 | ≤0.04 | ≤0.03 | ≤1 |
316L | 16-18 | 10-14 |
|
|
| ≤0.03 | ≤0.04 | ≤0.03 | ≤1 |
317L | 18-21 | 12-16 | 3-4 |
|
| ≤0.03 | ≤0.04 | ≤0.03 | ≤1 |
314 | 24-27 | 18-21 |
|
|
| ≤0.03 | ≤0.04 | ≤0.2 | 1.5/2.5 |
310 | 24-26 | 19-22 |
|
|
| ≤0.03 | ≤0.04 | ≤0.08 | ≤1 |
303LSC | 17-19 | 8-13 |
|
| 2 | 0.15-0.3 | ≤0.2 | ≤0.03 | ≤1 |
304LSC | 17-19 | 8-13 |
|
| 2 | ≤0.03 | ≤0.04 | ≤0.03 | ≤1 |
316LSC | 16-19 | 10-14 | 2-3 |
| 2 | ≤0.03 | ≤0.04 | ≤0.03 | ≤1 |
410L | 11.5-13.5 |
|
|
|
| ≤0.03 | ≤0.04 | ≤0.03 | ≤1 |
430L | 16-18 |
|
|
|
| ≤0.03 | ≤0.04 | ≤0.03 | ≤1 |
434L | 16-18 |
| 0.75-1.25 |
|
| ≤0.03 | ≤0.04 | ≤0.08 | ≤1 |
434LNB | 16-18 |
| 0.75-1.25 | 0.4-0.6 |
| ≤0.03 | ≤0.04 | ≤0.03 | ≤1 |
410 | 11.5-13.5 |
|
|
|
| ≤0.03 | ≤0.04 | ≤0.25 | ≤1 |
420 | 12-14 |
|
|
|
| ≤0.03 | ≤0.04 | 0.25/0.35 | ≤1 |
430 | 16-18 |
|
|
|
| ≤0.03 | ≤0.04 | ≤0.08 | ≤1 |
434 | 16-18 |
| 0.75-1.25 |
|
| ≤0.03 | ≤0.04 | ≤0.08 | ≤1 |
440 | 16-18 |
|
|
|
| ≤0.03 | ≤0.04 | 0.9/1.2 | ≤1 |
17-4PH | 15-17.5 | 3-5 |
| 0.15-0.456 | 3-5 | ≤0.03 | ≤0.04 | ≤0.07 | ≤1 |
15-5PH | 14-15.5 | 3.5-5.5 |
|
| 2.5-4.5 | ≤0.03 | ≤0.04 | <=0.07 | ≤1 |
Poud asye pur ka itilize pou flite tèmik, metaliji poud, metaliji poud laprès SINTERING (PM), bòdi piki (MIM) SINTERING filtre, elatriye, kontni oksijèn atomizasyon dlo.<4000PPM, atomizasyon gaz<1000PPM.
●Even poud konpozisyon, mwens impuretés
●High sphericity
●Low kontni oksijèn
●Good flowability
●High k'ap fè jennès dansite, wo tiyo dansite
●Less kre poud, mwens satelit poud
1.Huarui gen sistèm jesyon kalite strik.Nou teste pwodwi nou yo an premye apre nou fini pwodiksyon nou an, epi nou teste ankò anvan chak livrezon, menm echantiyon.Men, si ou bezwen, nou ta renmen aksepte twazyèm pati pou teste.Natirèlman si ou renmen, nou ta ka bay echantiyon pou ou teste.
2.Our bon jan kalite pwodwi garanti pa Sichuan Metallurgical Institute ak Guangzhou Institute of Metal Research.Koperasyon alontèm ak yo ka sove anpil tan tès pou kliyan yo.